One shrinkage percentage cannot describe every dimension of a molded component. Injection molding shrinkage depends on the resin grade, flow direction, local section, and the conditions under which the material cools and is measured. A supplier’s value is useful evidence, but it is not a promise that a housing, bore, and mounting pitch will all contract by the same amount.
The engineering task is to turn that evidence into an initial cavity allowance, identify where the assumption is uncertain, and check the result on trial parts. This article separates mold shrinkage from later dimensional movement and shows what should be agreed before a tool correction is authorized. It is not a guide to hiding sink marks with more holding pressure.
Begin with two dimensions and one measurement state
Linear mold shrinkage compares a mold cavity dimension with the corresponding dimension of a molded specimen or part under defined conditions. Volume shrinkage describes a different quantity. Mixing the two gives an apparent calculation with no reliable dimensional meaning. Establish which quantity a data sheet reports before using it to discuss a tool.
Also distinguish overall contraction from shape change. A panel can have the expected average length and still bow enough to miss its mating surface. A local depression behind a thick junction is another observation again. Shrinkage, warpage, and sink can be related through cooling and packing, but they are not interchangeable measurements or acceptance criteria.
Đối với một Ép phun nhựa project, record the dimension, datum scheme, material state, and measurement time alongside any shrinkage assumption. Without that context, two teams may report different dimensions while both have measured their samples correctly. The disagreement begins with the definition, not necessarily with the tool.
The arithmetic is simple; the allowance is not
Under a stated convention, linear shrinkage can be expressed as S = (Ltool − Lpart) / Ltool. Rearranging gives Ltool = Lpart / (1 − S). This relationship describes the arithmetic for that convention; it does not identify the correct shrinkage value for a complex part. An allowance must still reflect the intended resin, geometry, and processing evidence.
For an arithmetic example only, assume a target part length of 100 mm and an assumed linear shrinkage of 1%. The corresponding simple calculation gives about 101.01 mm for the tool dimension. Neither value describes a recommended allowance for an actual resin or component. The example demonstrates why the denominator and the definition of S must be clear.
A supplier’s test specimen can differ from the proposed part in flow length, thickness, gate arrangement, restraint, and cooling history. Record the specimen method and conditions when available, and ask how the proposed allowance was adjusted for the actual geometry. Avoid presenting the extra decimal places in a calculation as evidence that the underlying assumption is precise.
Toray’s AMILAN dimensional guidance distinguishes mold shrinkage from environmental and use-related dimensional changes. Its nylon-specific discussion also illustrates why thickness, molding conditions, and orientation matter. Use the relevant guidance for the actual grade; do not transfer a nylon-specific adjustment to unrelated polymers.
A housing does not shrink equally in every direction
Flow and reinforcement orientation can make dimensional response directional. The length along a major flow path, the width across it, and a dimension around a core may not behave alike. A single scale factor applied to the entire CAD model can conceal this difference. The mold designer needs to identify critical features, not merely enlarge the outside envelope.
Consider a hypothetical cover with a row of locating holes and a latch at one end. The buyer cares about the hole pitch and latch engagement, not just total length. Changes in gate location or local packing can affect those features differently. Comparing only the overall dimension can therefore approve a sample that still fails in assembly.

Build a dimensional map that relates critical features to the gate, section changes, and relevant cores. Where an analysis is used, record the material model and assumptions. Predictions can help prioritize trial measurements; they do not remove the need to measure the real features. Keep the proposed correction local where evidence supports a local issue rather than rescaling everything.
The part can keep moving after it leaves the mold
Cooling does not end all dimensional change. Depending on the polymer and its history, further structural change, temperature equilibration, moisture uptake, or release of residual stress may affect the part. These mechanisms need not act in the same direction. A dimension that changes later is not automatically proof that the initial cavity allowance was wrong.
Agree on the measurement condition that matters to the product. A dry molded nylon component and a conditioned component may not represent the same assembly state. Likewise, a warm part measured immediately after ejection should not be compared directly with a room-temperature inspection result without explaining the difference. Time, temperature, storage, and conditioning belong in the sample record.

| Dimension being compared | Missing condition that can mislead | Useful agreement |
|---|---|---|
| New sample against the drawing | Unspecified time after molding | Measurement timing and temperature |
| Dry part against a later assembly | Different moisture or storage state | Defined conditioning relevant to use |
| One cavity against another | Untracked cavity identity and process history | Cavity-specific traceability |
| Loose cover against an assembled cover | Different restraint and loading | Separate free-state and assembled checks |
The point is not to create unnecessary laboratory work. It is to avoid correcting a tool for a moving target. Use the product’s real fit and environment to choose the relevant state, then apply that state consistently across trials and later production approval.
Do not cut steel to correct an undefined measurement
Before changing cavity steel, confirm that the measured difference is repeatable and represents the condition the drawing intends. Review the measurement method, part support, cavity number, material identity, and process stability. A tool change may be appropriate, but it should follow evidence that the discrepancy belongs to the tool rather than a different sample state or unstable process.
Sử dụng một injection molding shrinkage measurement plan to separate the features that need correction from those already acceptable. Keep the measurement report connected to the CAD revision and trial conditions. If a tool change affects several related dimensions, identify them in advance and recheck them after the change.
- Verify the drawing requirement and how the part is located for measurement.
- Compare repeat samples with cavity and molding history recorded.
- Check the relevant conditioning or storage state before assigning the difference to shrinkage.
- Agree the correction, affected features, and repeat verification before machining.
Injection molding shrinkage is best treated as a documented design assumption that becomes better supported through trials. The final release should connect cavity revision, process conditions, measurement state, and functional fit. A statement that the tool uses a familiar percentage is not a substitute for that record.
Questions about shrinkage allowances
Can the molder use the material family’s average value?
It may be a preliminary screening value when better information is unavailable, but the uncertainty must be explicit. Confirm the exact grade, available supplier data, and critical dimensions before treating the allowance as ready for tooling.
Does increasing packing pressure solve every undersized dimension?
No. Packing affects the material state while pressure can still reach the region, but geometry, gate freeze, orientation, and later conditioning also matter. Review the mechanism rather than using one adjustment to compensate for an unexplained dimension.
Should the assembled part always match the free-state report?
Not necessarily. Assembly can constrain or load the component. Define which requirements apply in the free state and which apply in the assembly, so a forced fit is not mistaken for dimensional compliance.