{"id":2678,"date":"2026-07-25T17:18:58","date_gmt":"2026-07-25T09:18:58","guid":{"rendered":"http:\/\/0"},"modified":"2026-07-24T17:55:19","modified_gmt":"2026-07-24T09:55:19","slug":"understanding-injection-molding-bayblend-fr3010-for-ev-battery-modules","status":"publish","type":"post","link":"https:\/\/www.jcinjectionmolding.com\/fr\/blog\/understanding-injection-molding-bayblend-fr3010-for-ev-battery-modules\/","title":{"rendered":"Comprendre le moulage par injection Bayblend FR3010 pour les modules de batterie de v\u00e9hicules \u00e9lectriques"},"content":{"rendered":"<article style=\", Roboto, Helvetica, Arial, sans-serif;color: #333333;width: 100%\">\n<section style=\"margin-bottom: 30px\">\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 24px\">Les syst\u00e8mes de batteries haute performance pour v\u00e9hicules \u00e9lectriques (VE) n\u00e9cessitent des bo\u00eetiers en mat\u00e9riaux avanc\u00e9s.<br \/>\nLa s\u00e9lection de la r\u00e9sine technique appropri\u00e9e joue un r\u00f4le essentiel pour \u00e9quilibrer la t\u00e9nacit\u00e9 structurelle et la rigidit\u00e9 di\u00e9lectrique \u00e9lev\u00e9e.<br \/>\nLe Covestro Bayblend FR3010 s'est impos\u00e9 comme une r\u00e9f\u00e9rence industrielle pour le moulage de composants de batterie hautement int\u00e9gr\u00e9s.<br \/>\nLa transformation de ce m\u00e9lange PC\/ABS ignifuge et sans halog\u00e8ne exige un contr\u00f4le strict de la temp\u00e9rature et du cisaillement.<br \/>\nCette fiche technique et ce guide de transformation d\u00e9taillent les param\u00e8tres de moulage essentiels, les exigences d'\u00e9ventage et les strat\u00e9gies de pr\u00e9vention de la d\u00e9gradation n\u00e9cessaires pour produire des pi\u00e8ces fiables.<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-2680\" src=\"https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/raw-plastic-material-hopper-feed.webp\" alt=\"raw-plastic-material-hopper-feed\" width=\"1376\" height=\"768\" srcset=\"https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/raw-plastic-material-hopper-feed.webp 1376w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/raw-plastic-material-hopper-feed-300x167.webp 300w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/raw-plastic-material-hopper-feed-1024x572.webp 1024w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/raw-plastic-material-hopper-feed-768x429.webp 768w\" sizes=\"auto, (max-width: 1376px) 100vw, 1376px\" \/><\/p>\n<\/section>\n<p><!-- Table of Contents --><\/p>\n<section style=\"background-color: #f8f9fa;border-left: 4px solid #0056b3;padding: 24px;border-radius: 6px;margin: 40px 0\">\n<h3 style=\"font-size: 22px;font-weight: bold;line-height: 1.5em;margin-top: 0;margin-bottom: 16px;color: #111111\">Table des mati\u00e8res<\/h3>\n<ul style=\"list-style-type: none;padding-left: 0;margin: 0\">\n<li style=\"margin-bottom: 12px\"><a style=\"color: #0056b3;text-decoration: none;font-size: 17px;font-weight: 500\" href=\"#preferred-material\">1. Pourquoi le Covestro Bayblend FR3010 est privil\u00e9gi\u00e9 pour les composants de batterie<\/a><\/li>\n<li style=\"margin-bottom: 12px\"><a style=\"color: #0056b3;text-decoration: none;font-size: 17px;font-weight: 500\" href=\"#molding-parameters\">2. Param\u00e8tres techniques de moulage pour le Bayblend FR3010<\/a><\/li>\n<li style=\"margin-bottom: 0\"><a style=\"color: #0056b3;text-decoration: none;font-size: 17px;font-weight: 500\" href=\"#tooling-venting\">3. Conseils de conception d'outillage et d'\u00e9ventage pour pr\u00e9venir la d\u00e9gradation des retardateurs de flamme<\/a><\/li>\n<\/ul>\n<\/section>\n<p><!-- Section 1 --><\/p>\n<section id=\"preferred-material\" style=\"margin-bottom: 50px\">\n<h2 style=\"font-size: 28px;line-height: 1.5em;font-weight: bold;margin-top: 40px;margin-bottom: 24px;color: #111111;border-bottom: 1px solid #eaeaea;padding-bottom: 8px\">Pourquoi le Covestro Bayblend FR3010 est privil\u00e9gi\u00e9 pour les composants de batterie<\/h2>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-2679\" src=\"https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/plastic-impact-strength-laboratory-test.webp\" alt=\"plastic-impact-strength-laboratory-test\" width=\"1376\" height=\"768\" srcset=\"https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/plastic-impact-strength-laboratory-test.webp 1376w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/plastic-impact-strength-laboratory-test-300x167.webp 300w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/plastic-impact-strength-laboratory-test-1024x572.webp 1024w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/plastic-impact-strength-laboratory-test-768x429.webp 768w\" sizes=\"auto, (max-width: 1376px) 100vw, 1376px\" \/><\/p>\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 24px\">Le Covestro Bayblend FR3010 offre un profil \u00e9quilibr\u00e9 de r\u00e9sistance aux chocs, de fluidit\u00e9 et de conformit\u00e9 en mati\u00e8re de s\u00e9curit\u00e9.<br \/>\nLes retardateurs de flamme sans halog\u00e8ne sont respectueux de l'environnement et r\u00e9pondent aux directives europ\u00e9ennes strictes REACH\/RoHS.<br \/>\nLa conception de composants structurels avec cette nuance PC\/ABS permet de pr\u00e9venir les d\u00e9faillances m\u00e9caniques localis\u00e9es.<br \/>\nPlus pr\u00e9cis\u00e9ment, une expertise en <strong>moulage par injection Bayblend FR3010 pour modules de batterie EV<\/strong> garantit des propri\u00e9t\u00e9s physiques hautement stables.<\/p>\n<p><!-- Bulleted List (\u5c0f\u5706\u70b9\u533a\u5206\u5206\u7c7b) --><\/p>\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 16px\">Les principaux avantages des mat\u00e9riaux incluent :<\/p>\n<ul style=\"font-size: 18px;line-height: 1.8em;margin-bottom: 24px;padding-left: 24px;list-style-type: disc\">\n<li style=\"margin-bottom: 12px;text-align: left\"><strong>Haute r\u00e9sistance aux chocs<\/strong>\u2014Le PC\/ABS amorphe offre un excellent comportement ductile jusqu'\u00e0 basse temp\u00e9rature.<\/li>\n<li style=\"margin-bottom: 12px;text-align: left\"><strong>Ignifugation<\/strong>\u2014Des additifs sans halog\u00e8ne permettent d'atteindre une classification de s\u00e9curit\u00e9 UL94 V-0 pour des \u00e9paisseurs de paroi de 1,5 mm.<\/li>\n<li style=\"margin-bottom: 12px;text-align: left\"><strong>Viscosit\u00e9 optimale<\/strong>\u2014Un bon comportement d'\u00e9coulement permet le remplissage de porte-cellules structurels complexes \u00e0 plusieurs empreintes.<\/li>\n<li style=\"margin-bottom: 12px;text-align: left\"><strong>Ma\u00eetrise dimensionnelle<\/strong>\u2014Un retrait pr\u00e9visible limite le gauchissement structurel des couvercles sup\u00e9rieurs d'enceinte plats.<\/li>\n<\/ul>\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 24px\">Un comportement m\u00e9canique \u00e9quilibr\u00e9 est crucial lors d'\u00e9v\u00e9nements thermiques haute tension.<br \/>\nCette nuance r\u00e9siste \u00e0 la propagation sous vibration structurelle continue, maintenant les cellules cylindriques isol\u00e9es en toute s\u00e9curit\u00e9.<br \/>\nPar cons\u00e9quent, les cadres polym\u00e8res conservent leurs distances d'isolement \u00e9lectrique lors des essais dynamiques sur v\u00e9hicule.<\/p>\n<\/section>\n<p><!-- Section 2 --><\/p>\n<section id=\"molding-parameters\" style=\"margin-bottom: 50px\">\n<h2 style=\"font-size: 28px;line-height: 1.5em;font-weight: bold;margin-top: 40px;margin-bottom: 24px;color: #111111;border-bottom: 1px solid #eaeaea;padding-bottom: 8px\">Param\u00e8tres techniques de moulage pour Bayblend FR3010<\/h2>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-2683\" src=\"https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/injection-molding-controller-display-parameters.webp\" alt=\"injection-molding-controller-display-parameters\" width=\"1376\" height=\"768\" srcset=\"https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/injection-molding-controller-display-parameters.webp 1376w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/injection-molding-controller-display-parameters-300x167.webp 300w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/injection-molding-controller-display-parameters-1024x572.webp 1024w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/injection-molding-controller-display-parameters-768x429.webp 768w\" sizes=\"auto, (max-width: 1376px) 100vw, 1376px\" \/><\/p>\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 24px\">La mise en \u0153uvre de cette r\u00e9sine technique exige des param\u00e8tres pr\u00e9cis.<br \/>\nUne mise en \u0153uvre r\u00e9ussie <strong>moulage par injection Bayblend FR3010 pour modules de batterie EV<\/strong> exige une masse plastique propre et exempte d'humidit\u00e9.<br \/>\nL'absorption d'humidit\u00e9 provoque des d\u00e9fauts esth\u00e9tiques tels que des marques de splay, tout en d\u00e9gradant chimiquement les cha\u00eenes polym\u00e8res.<br \/>\nPar cons\u00e9quent, les s\u00e9cheurs \u00e0 tr\u00e9mie \u00e0 roue dessiccative doivent s\u00e9cher les granul\u00e9s bruts jusqu'\u00e0 une teneur en humidit\u00e9 inf\u00e9rieure \u00e0 0,02 %.<\/p>\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 24px\">Pour \u00e9viter le placage de surface et les contraintes r\u00e9siduelles, les temp\u00e9ratures de moule doivent \u00eatre maintenues entre 70\u00b0C et 90\u00b0C.<br \/>\nLe maintien de temp\u00e9ratures de mati\u00e8re fondu correctes emp\u00eache le cisaillement mol\u00e9culaire tout en pr\u00e9servant les performances ignifuges.<br \/>\nL'ajustement dynamique des vitesses d'injection pendant le remplissage de la cavit\u00e9 garantit une densit\u00e9 uniforme.<\/p>\n<p><!-- Molding Parameter Table --><\/p>\n<div style=\"margin: 32px 0\">\n<table style=\"width: 100%;border-collapse: collapse;font-size: 16px;text-align: left;min-width: 600px\">\n<thead>\n<tr style=\"background-color: #f8f9fa;border-bottom: 2px solid #dee2e6\">\n<th style=\"padding: 16px;border: 1px solid #dee2e6;font-weight: 600;color: #111111\">Type de param\u00e8tre<\/th>\n<th style=\"padding: 16px;border: 1px solid #dee2e6;font-weight: 600;color: #111111\">R\u00e9glage cible<\/th>\n<th style=\"padding: 16px;border: 1px solid #dee2e6;font-weight: 600;color: #111111\">Plage op\u00e9rationnelle<\/th>\n<th style=\"padding: 16px;border: 1px solid #dee2e6;font-weight: 600;color: #111111\">Point de contr\u00f4le critique<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr style=\"border-bottom: 1px solid #dee2e6\">\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">Temp\u00e9rature de s\u00e9chage<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">100\u00b0C<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">95\u00b0C \u2013 105\u00b0C<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">Utiliser une roue d\u00e9shydratante, s\u00e9cher pendant 4 heures.<\/td>\n<\/tr>\n<tr style=\"border-bottom: 1px solid #dee2e6\">\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">Temp\u00e9rature de fusion<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">270\u00b0C<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">260\u00b0C \u2013 280\u00b0C<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">\u00c9viter de d\u00e9passer 290\u00b0C pour pr\u00e9venir la d\u00e9gradation des additifs.<\/td>\n<\/tr>\n<tr style=\"border-bottom: 1px solid #dee2e6\">\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">Temp\u00e9rature du moule<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">80\u00b0C<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">70 \u00b0C \u2013 90 \u00b0C<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">Utilisez un chauffage \u00e0 l'eau chaude pour r\u00e9duire les contraintes.<\/td>\n<\/tr>\n<tr style=\"border-bottom: 1px solid #dee2e6\">\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">Pression d'injection<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">100 MPa<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">80 \u2013 120 MPa<\/td>\n<td style=\"padding: 16px;border: 1px solid #dee2e6;color: #333333\">Surveillez les capteurs de cavit\u00e9 en temps r\u00e9el.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<\/section>\n<p><!-- Section 3 --><\/p>\n<section id=\"tooling-venting\" style=\"margin-bottom: 50px\">\n<h2 style=\"font-size: 28px;line-height: 1.5em;font-weight: bold;margin-top: 40px;margin-bottom: 24px;color: #111111;border-bottom: 1px solid #eaeaea;padding-bottom: 8px\">Conseils de conception d'outillage et d'\u00e9ventage pour pr\u00e9venir la d\u00e9gradation des retardateurs de flamme<\/h2>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-2682\" src=\"https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/high-precision-mold-venting-channels.webp\" alt=\"high-precision-mold-venting-channels\" width=\"1376\" height=\"768\" srcset=\"https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/high-precision-mold-venting-channels.webp 1376w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/high-precision-mold-venting-channels-300x167.webp 300w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/high-precision-mold-venting-channels-1024x572.webp 1024w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/high-precision-mold-venting-channels-768x429.webp 768w\" sizes=\"auto, (max-width: 1376px) 100vw, 1376px\" \/><\/p>\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 24px\">Les concepteurs de moules doivent accorder une attention particuli\u00e8re \u00e0 l'\u00e9ventage et \u00e0 la g\u00e9om\u00e9trie des seuils d'injection.<br \/>\nLes additifs retardateurs de flamme se d\u00e9gradent lorsqu'ils sont expos\u00e9s \u00e0 un cisaillement extr\u00eame ou \u00e0 une surchauffe localis\u00e9e.<br \/>\nCette d\u00e9gradation lib\u00e8re des gaz acides qui corrodent les aciers de moule de haute qualit\u00e9.<br \/>\nPar cons\u00e9quent, les param\u00e8tres d\u00e9licats de <strong>moulage par injection Bayblend FR3010 pour modules de batterie EV<\/strong> n\u00e9cessitent des sections transversales de seuil d'injection optimis\u00e9es.<\/p>\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 24px\">Les seuils \u00e0 pointe et autres types de seuils tr\u00e8s restrictifs g\u00e9n\u00e8rent une chaleur de frottement excessive.<br \/>\nL'utilisation de seuils \u00e0 languette ou de seuils en \u00e9ventail r\u00e9partit uniform\u00e9ment la pression de la mati\u00e8re fondue, ce qui pr\u00e9vient la d\u00e9gradation du mat\u00e9riau.<br \/>\nNos recommandations d'outillage comprennent :<\/p>\n<p><!-- Numbered List (\u5e8f\u53f7\u533a\u5206\u6d41\u7a0b) --><\/p>\n<ol style=\"font-size: 18px;line-height: 1.8em;margin-bottom: 24px;padding-left: 24px;list-style-type: decimal\">\n<li style=\"margin-bottom: 12px;text-align: left\"><strong>Optimisation du diam\u00e8tre de la carotte<\/strong>\u2014Garantir des sections transversales de carotte g\u00e9n\u00e9reuses permet d'\u00e9viter un \u00e9chauffement par cisaillement excessif pendant la phase d'injection \u00e0 haute pression.<\/li>\n<li style=\"margin-bottom: 12px;text-align: left\"><strong>Fentes d'\u00e9ventation des gaz<\/strong>\u2014L'int\u00e9gration de canaux d'\u00e9ventation le long du plan de joint emp\u00eache l'emprisonnement des gaz, pr\u00e9servant ainsi la chimie intacte du mat\u00e9riau.<\/li>\n<li style=\"margin-bottom: 12px;text-align: left\"><strong>Rev\u00eatement de surface de l'empreinte<\/strong>\u2014L'application d'un chromage ou d'un d\u00e9p\u00f4t physique en phase vapeur prot\u00e8ge l'outil d'empreinte du d\u00e9gazage acide des retardateurs de flamme.<\/li>\n<li style=\"margin-bottom: 12px;text-align: left\"><strong>R\u00e9seaux de refroidissement du noyau<\/strong>\u2014L'optimisation des circuits d'\u00e9coulement d'eau permet d'\u00e9viter les points chauds localis\u00e9s susceptibles de d\u00e9clencher une d\u00e9gradation du polym\u00e8re.<\/li>\n<\/ol>\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 24px\">En d\u00e9finitive, nous appliquons avec succ\u00e8s notre exp\u00e9rience en <strong>moulage par injection Bayblend FR3010 pour modules de batterie EV<\/strong> lors de la fabrication de <strong>bo\u00eetiers de batterie en plastique sur mesure pour v\u00e9hicules \u00e9lectriques<\/strong>.<br \/>\nCette ex\u00e9cution technique compl\u00e8te minimise les d\u00e9faillances des composants en aval.<br \/>\nEn combinant l'outillage de pr\u00e9cision avec des syst\u00e8mes de qualit\u00e9 certifi\u00e9s IATF 16949, JUCHENG propose des solutions de fabrication fiables.<\/p>\n<\/section>\n<p><!-- Section 5: FAQ --><\/p>\n<section id=\"faq\" style=\"margin-bottom: 40px\">\n<h2 style=\"font-size: 28px;line-height: 1.5em;font-weight: bold;margin-top: 40px;margin-bottom: 24px;color: #111111;border-bottom: 1px solid #eaeaea;padding-bottom: 8px\">Questions fr\u00e9quemment pos\u00e9es (FAQ)<\/h2>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-2684\" src=\"https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/inspecting-pc-abs-molded-part.webp\" alt=\"inspecting-pc-abs-molded-part\" width=\"1376\" height=\"768\" srcset=\"https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/inspecting-pc-abs-molded-part.webp 1376w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/inspecting-pc-abs-molded-part-300x167.webp 300w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/inspecting-pc-abs-molded-part-1024x572.webp 1024w, https:\/\/www.jcinjectionmolding.com\/wp-content\/uploads\/2026\/07\/inspecting-pc-abs-molded-part-768x429.webp 768w\" sizes=\"auto, (max-width: 1376px) 100vw, 1376px\" \/><\/p>\n<div style=\"margin-bottom: 30px\">\n<h3 style=\"font-size: 22px;line-height: 1.5em;font-weight: bold;margin-top: 24px;margin-bottom: 12px;color: #111111\">Pourquoi le Bayblend FR3010 n\u00e9cessite-t-il un d\u00e9shydrateur \u00e0 dessiccant plut\u00f4t qu'un s\u00e9cheur \u00e0 air chaud ?<\/h3>\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 24px\">Les s\u00e9cheurs \u00e0 roue dessiccante offrent un point de ros\u00e9e de -40 \u00b0C, essentiel pour capturer l'humidit\u00e9 ambiante dans le PC\/ABS.<br \/>\nLes s\u00e9cheurs \u00e0 air chaud se contentent de faire circuler de l'air humide, sans parvenir \u00e0 extraire l'eau de la structure mol\u00e9culaire.<br \/>\nUn s\u00e9chage appropri\u00e9 emp\u00eache le clivage hydrolytique pendant la phase de fusion, pr\u00e9servant ainsi la r\u00e9sistance aux chocs.<\/p>\n<\/div>\n<div style=\"margin-bottom: 30px\">\n<h3 style=\"font-size: 22px;line-height: 1.5em;font-weight: bold;margin-top: 24px;margin-bottom: 12px;color: #111111\">Comment pr\u00e9venir les marques de splay sur la surface de la pi\u00e8ce ?<\/h3>\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 24px\">Les marques de splay sont caus\u00e9es par l'humidit\u00e9 de surface ou la surchauffe.<br \/>\nMaintenir la limite d'humidit\u00e9 en dessous de 0,02 % est la premi\u00e8re \u00e9tape critique.<br \/>\nDe plus, ralentir la vitesse d'injection initiale emp\u00eache le splay d\u00fb au cisaillement par frottement sur les parois de l'empreinte.<\/p>\n<\/div>\n<div style=\"margin-bottom: 0\">\n<h3 style=\"font-size: 22px;line-height: 1.5em;font-weight: bold;margin-top: 24px;margin-bottom: 12px;color: #111111\">Quel acier \u00e0 outils est recommand\u00e9 pour les compounds PC\/ABS FR corrosifs ?<\/h3>\n<p style=\"font-size: 18px;line-height: 1.8em;text-align: left;margin-bottom: 24px\">Les d\u00e9gagements gazeux corrosifs n\u00e9cessitent des aciers inoxydables de qualit\u00e9 sup\u00e9rieure comme le S136 tremp\u00e9 \u00e0 HRC 48-52.<br \/>\nCet acier offre une r\u00e9sistance sup\u00e9rieure aux d\u00e9gagements gazeux de phosphore corrosif.<br \/>\nNous recommandons \u00e9galement le chromage de la face du moule pour les productions \u00e0 tr\u00e8s grand volume.<\/p>\n<\/div>\n<\/section>\n<\/article>","protected":false},"excerpt":{"rendered":"<p>High-performance electric vehicle (EV) battery systems require advanced material housings. Selecting the correct engineering resin plays a vital role in balancing structural toughness and high dielectric strength. Covestro Bayblend FR3010 has emerged as an industry standard for molding highly integrated battery components. Processing this halogen-free, flame-retardant PC\/ABS blend demands strict control over temperature and shear. [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":2681,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1],"tags":[],"class_list":["post-2678","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-blog"],"_links":{"self":[{"href":"https:\/\/www.jcinjectionmolding.com\/fr\/wp-json\/wp\/v2\/posts\/2678","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jcinjectionmolding.com\/fr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.jcinjectionmolding.com\/fr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.jcinjectionmolding.com\/fr\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/www.jcinjectionmolding.com\/fr\/wp-json\/wp\/v2\/comments?post=2678"}],"version-history":[{"count":0,"href":"https:\/\/www.jcinjectionmolding.com\/fr\/wp-json\/wp\/v2\/posts\/2678\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.jcinjectionmolding.com\/fr\/wp-json\/wp\/v2\/media\/2681"}],"wp:attachment":[{"href":"https:\/\/www.jcinjectionmolding.com\/fr\/wp-json\/wp\/v2\/media?parent=2678"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.jcinjectionmolding.com\/fr\/wp-json\/wp\/v2\/categories?post=2678"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.jcinjectionmolding.com\/fr\/wp-json\/wp\/v2\/tags?post=2678"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}